Massive porosity on my starts. One mm bubble(or two) on surface, but nickle-size cluster underneath after grinding. Once every 4 rods. ESAB 5mm and 6mm, 7018.
About 1000" of piping production so far. 16" sch60.
Going to try Liquid Air. Don't know what else to do.
Suggestions...